Production of Gold - West Virginia University
2016-8-1 · gold at 1300°C, with fluxes of silica, feldspar, and borax, to remove impurities. Complete separation occurs within 1.5 hours, at which point the slag is poured off and the molten gold is poured into anode casts and cooled. The anodes are approximately 99% pure and are submerged with 99.9% pure rolled gold cathodes in an electrolytic solution